Zn-Cu Alloy Nanofoams as Efficient Catalysts for the Reduction of CO

CO2 reduction alloys electrocatalysis electrolysis syngas

Journal

ChemSusChem
ISSN: 1864-564X
Titre abrégé: ChemSusChem
Pays: Germany
ID NLM: 101319536

Informations de publication

Date de publication:
24 Jan 2019
Historique:
received: 05 10 2018
revised: 13 11 2018
pubmed: 15 1 2019
medline: 15 1 2019
entrez: 15 1 2019
Statut: ppublish

Résumé

Alloying strategies are commonly used to design electrocatalysts that take on properties of their constituent elements. Herein, such a strategy is used to develop Zn-Cu alloyed electrodes with unique hierarchical porosity and tunable selectivity for CO

Identifiants

pubmed: 30637969
doi: 10.1002/cssc.201802287
doi:

Types de publication

Journal Article

Langues

eng

Pagination

511-517

Informations de copyright

© 2019 Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim.

Auteurs

Sarah Lamaison (S)

Laboratoire de Chimie des Processus Biologiques, CNRS UMR 8229, Collège de France, Sorbonne Université, 11 Place Marcelin Berthelot, 75231, Paris Cedex 05, France.

David Wakerley (D)

Laboratoire de Chimie des Processus Biologiques, CNRS UMR 8229, Collège de France, Sorbonne Université, 11 Place Marcelin Berthelot, 75231, Paris Cedex 05, France.

David Montero (D)

Institut des Matériaux de Paris Centre, FR 2482, Sorbonne Université, 4 place Jussieu, 75005, Paris, France.

Gwenaëlle Rousse (G)

Laboratoire de Chimie du Solide et Energie, UMR 8260, Collège de France, Sorbonne Université, 11 Place Marcelin Berthelot, 75231, Paris Cedex 05, France.

Dario Taverna (D)

Institut de Minéralogie, de Physique des Matériaux et de Cosmochimie, CNRS UMR 7590, MNHN, IRD, Sorbonne Université, 4 place Jussieu, 75005, Paris, France.

Domitille Giaume (D)

Chimie ParisTech, PSL Research University, CNRS, Institut de Recherche de Chimie de Paris, 11 rue Pierre et Marie Curie, 75005, Paris, France.

Dimitri Mercier (D)

Chimie ParisTech, PSL Research University, CNRS, Institut de Recherche de Chimie de Paris, 11 rue Pierre et Marie Curie, 75005, Paris, France.

Juliette Blanchard (J)

Sorbonne Université, CNRS, Laboratoire de Réactivité de Surface, LRS UMR 7197, 75005, Paris, France.

Huan Ngoc Tran (HN)

Laboratoire de Chimie des Processus Biologiques, CNRS UMR 8229, Collège de France, Sorbonne Université, 11 Place Marcelin Berthelot, 75231, Paris Cedex 05, France.

Marc Fontecave (M)

Laboratoire de Chimie des Processus Biologiques, CNRS UMR 8229, Collège de France, Sorbonne Université, 11 Place Marcelin Berthelot, 75231, Paris Cedex 05, France.

Victor Mougel (V)

Laboratoire de Chimie des Processus Biologiques, CNRS UMR 8229, Collège de France, Sorbonne Université, 11 Place Marcelin Berthelot, 75231, Paris Cedex 05, France.
Current address: Department of Chemistry and Applied Biosciences, Laboratory of Inorganic Chemistry, Swiss Federal Institute of Technology Zürich, Valdimir-Prelog-Weg 1, 8093, Zürich, Switzerland.

Classifications MeSH