Colored Janus Nanocylinders Driven by Supramolecular Coassembly of Donor and Acceptor Building Blocks.

1D structures Janus particles charge transfer complex hydrogen bonds nanoparticles rods self-assembly

Journal

ACS nano
ISSN: 1936-086X
Titre abrégé: ACS Nano
Pays: United States
ID NLM: 101313589

Informations de publication

Date de publication:
23 Feb 2021
Historique:
pubmed: 30 1 2021
medline: 30 1 2021
entrez: 29 1 2021
Statut: ppublish

Résumé

Janus nanocylinders exhibit nanometric dimensions, a high aspect ratio, and two faces with different chemistries (Janus character), making them potentially relevant for applications in optics, magnetism, catalysis, surface nanopatterning, or interface stabilization, but they are also very difficult to prepare by conventional strategies. In the present work, Janus nanocylinders were prepared by supramolecular coassembly in water of two different polymers functionalized with complementary assembling units. The originality of our approach consists in combining charge transfer complexation between electron-rich and electron-poor units with hydrogen bonding to (1) drive the supramolecular formation of one-dimensional structures (cylinders), (2) force the two polymer arms on opposite sides of the cylinders independently of their compatibility, resulting in Janus nanoparticles, and (3) detect coassembly through a color change of the solution upon mixing of the functional polymers.

Identifiants

pubmed: 33512151
doi: 10.1021/acsnano.0c07039
doi:

Types de publication

Journal Article

Langues

eng

Sous-ensembles de citation

IM

Pagination

2569-2577

Auteurs

Thomas Choisnet (T)

Institut des Molécules et Matériaux du Mans (IMMM), UMR 6283 CNRS, Le Mans Université, Avenue Olivier Messiaen, 72085 Le Mans, Cedex 9, France.
Laboratoire MOLTECH-Anjou, UNIV Angers, SFR MATRIX, UMR CNRS 6200, 2 Bd Lavoisier, 49045 Angers Cedex, France.

David Canevet (D)

Laboratoire MOLTECH-Anjou, UNIV Angers, SFR MATRIX, UMR CNRS 6200, 2 Bd Lavoisier, 49045 Angers Cedex, France.

Marc Sallé (M)

Laboratoire MOLTECH-Anjou, UNIV Angers, SFR MATRIX, UMR CNRS 6200, 2 Bd Lavoisier, 49045 Angers Cedex, France.

Cédric Lorthioir (C)

CNRS, Laboratoire de Chimie de la Matière Condensée de Paris, Sorbonne Université, UMR 7574, 75252 Paris, France.

Laurent Bouteiller (L)

CNRS, Institut Parisien de Chimie Moléculaire, Sorbonne Université, UMR 8232, Equipe Chimie des Polymères, 75252 Paris, France.

Patrice Woisel (P)

Univ. Lille, CNRS, INRAE, Centrale Lille, UMR 8207 - UMET - Unité Matériaux et Transformations, F-59000 Lille, France.

Frédérick Niepceron (F)

Institut des Molécules et Matériaux du Mans (IMMM), UMR 6283 CNRS, Le Mans Université, Avenue Olivier Messiaen, 72085 Le Mans, Cedex 9, France.

Erwan Nicol (E)

Institut des Molécules et Matériaux du Mans (IMMM), UMR 6283 CNRS, Le Mans Université, Avenue Olivier Messiaen, 72085 Le Mans, Cedex 9, France.

Olivier Colombani (O)

Institut des Molécules et Matériaux du Mans (IMMM), UMR 6283 CNRS, Le Mans Université, Avenue Olivier Messiaen, 72085 Le Mans, Cedex 9, France.

Classifications MeSH