Investigation of MAO Coatings Characteristics on Titanium Products Obtained by EBM Method Using Additive Manufacturing.
MAO coating
additive manufacturing
composition
electron beam melting
heat resistance
micro-arc oxidation
roughness
structure
surface morphology
thermal cycling test
thickness
titanium alloy Ti-6Al-4V
Journal
Materials (Basel, Switzerland)
ISSN: 1996-1944
Titre abrégé: Materials (Basel)
Pays: Switzerland
ID NLM: 101555929
Informations de publication
Date de publication:
28 Jun 2022
28 Jun 2022
Historique:
received:
27
05
2022
revised:
24
06
2022
accepted:
25
06
2022
entrez:
9
7
2022
pubmed:
10
7
2022
medline:
10
7
2022
Statut:
epublish
Résumé
Coatings with a thickness from 27 to 62 µm on electron beam melted Ti-6Al-4V have been formed by micro-arc oxidation (MAO) in a silicate-hypophosphite electrolyte. MAO tests in the anode-cathode mode (50 Hz) with an anode-to-cathode current ratio of 1:1 and sum current densities 10 and 20 A/dm
Identifiants
pubmed: 35806660
pii: ma15134535
doi: 10.3390/ma15134535
pmc: PMC9267494
pii:
doi:
Types de publication
Journal Article
Langues
eng
Subventions
Organisme : Russian Science Foundation
ID : 21 -79-30058
Références
Periodontol 2000. 2017 Feb;73(1):22-40
pubmed: 28000277
Materials (Basel). 2019 Dec 01;12(23):
pubmed: 31805644
J Mater Sci Mater Med. 2010 Jan;21(1):259-66
pubmed: 19641851
Heliyon. 2021 May 07;7(5):e06892
pubmed: 34027149
Biomedicines. 2021 Dec 17;9(12):
pubmed: 34944750
Materials (Basel). 2021 Jan 03;14(1):
pubmed: 33401601
Mater Sci Eng C Mater Biol Appl. 2019 Sep;102:844-862
pubmed: 31147056