Design and development of keratin/chitosan/glucosamine sulfate composite loaded MWCNT intended for osteoarthritis drug delivery.
MWCNT
docking
drug delivery
glucosamine sulfate
keratin
nanoparticles
osteoarthritis
Journal
Biomedical materials (Bristol, England)
ISSN: 1748-605X
Titre abrégé: Biomed Mater
Pays: England
ID NLM: 101285195
Informations de publication
Date de publication:
30 05 2023
30 05 2023
Historique:
received:
21
11
2022
accepted:
18
05
2023
medline:
31
5
2023
pubmed:
19
5
2023
entrez:
18
5
2023
Statut:
epublish
Résumé
Osteoarthritis (OA) is an inflammatory disease that affects the cartilage and tissues around the joints, which results in excessive pain and stiffness. One of the most critical challenges for improving the therapeutic effect in OA treatments is the current drug design utilizing functional polymers. Indeed, there is a need to design and develop novel therapeutic drugs for positive outcomes. In this view, glucosamine sulfate is a drug used to manage OA because of its potential therapeutic effects on cartilage and ability to inhibit disease progression. This research aims to develop a keratin/chitosan/glucosamine sulfate (KRT/CS/GLS) composite loaded functionalized multi-walled carbon nanotubes (MWCNTs) as a potential carrier for the treatment of OA. The nanocomposite was developed using various ratios of KRT/CS/GLS, and MWCNT. Molecular docking analysis has been performed with (D-glucosamine) and targeted proteins (Protein Data Bank ID: 1HJV, 1ALU) to determine the binding affinity and interactions. Field emission scanning electron microscopy study showed that the composite KRT/CS/GLS incorporated on the surface of functionalized MWCNTs effectively. Fourier transform infrared spectroscopy analysis confirmed the presence of KRT/CS/GLS in the nanocomposite and remained intact. X-ray diffraction analysis indicated that the nature of the composite in MWCNT transformed from a crystalline to an amorphous state. Thermo gravimetric analysis revealed that the nanocomposite has a high thermal decomposition temperature of 420 °C. The MTT assay results showed that 83% of cell viability has remained in RAW 264.7 cells at the maximum concentration (500 μg ml
Identifiants
pubmed: 37201514
doi: 10.1088/1748-605X/acd6c9
doi:
Substances chimiques
Chitosan
9012-76-4
Glucosamine
N08U5BOQ1K
Keratins
68238-35-7
Nanotubes, Carbon
0
Types de publication
Journal Article
Langues
eng
Sous-ensembles de citation
IM
Informations de copyright
© 2023 IOP Publishing Ltd.